Skip to McMaster Navigation Skip to Site Navigation Skip to main content

Mystery solved: Researchers discover why zinc-ion batteries experience ‘capacity fade’

Engineering PhD grad Caio Miliante combined computational modelling and real-time experiments for his findings, which pave the way for better battery designs.

By Jesse Dorey, Faculty of Engineering October 23, 2026

A wind energy farm with tall turbines on a sunny day.
Zinc-ion batteries are considered one of the most promising options for storing renewable energy generated by wind or solar.

Experts Featured In This Story

Drew Higgins
Drew Higgins

Associate Professor

See Profile
Oleg Rubel
Oleg Rubel

Associate Professor

See Profile

With power demands growing across the world, researchers are searching for ways to efficiently and effectively store energy generated by renewable sources, such as wind and solar.

Zinc-ion batteries are considered one of the most promising alternatives for renewable energy storage. Unlike commonly used lithium-ion batteries, these are non-flammable, can operate efficiently across a wide range of temperatures and are easier to recycle, making them cheaper, safer and more sustainable.

But zinc-ion batteries have a tendency to lose the ability to store energy over repeated charge and discharge cycles.

“I would say the only reason we’re not using them right now is because we suffer so much with the capacity fade that they have,” explains Caio Miliante, a former PhD student co-supervised by Chemical Engineering professor Drew Higgins and Materials Science and Engineering professor Oleg Rubel.

In a recent study published in EES Batteries, Miliante, working with Salient Energy Inc., combined predictive computational modelling with nuclear magnetic resonance to better understand how the materials behave inside the battery and why they are susceptible to capacity fade.

Capacity fade at an atomic level

Miliante’s study focused on manganese dioxide, a material used in the cathode — a part of the battery involved with storing and releasing electrical energy — in rechargeable zinc-ion batteries.

During the discharge phase, explains Miliante, zinc ions enter the cathode and promote the structural dissolution. This was a commonly known issue with zinc-ion batteries, but Miliante wanted to know why it was happening.

Using predictive computer modelling, Miliante investigated what happens to the material when a manganese atom left the structure.

The calculations revealed that once zinc atoms enter the structure, they push the manganese atoms out of their usual positions. Once this vacancy forms, the nearby zinc atoms move into the now-vacant manganese sites and establish a more stable coordination within the cathode structure that makes it easier for manganese to dissolve into the liquid electrolytes inside the battery.

This loss, says Miliante, destabilizes the structure and contributes to capacity fade.

Computational modelling + real-time experiments

Miliante’s computational findings were paired with nuclear magnetic resonance experiments, a real-time technique that uses non-invasive imaging to monitor chemical reactions and material changes in a cell.

These experiments, conducted with Gillian Goward’s group from the Faculty of Science, allowed the researchers to track manganese while the battery was operating.

The measurements supported the computational findings, showing that manganese was in fact dissolving during the discharge phase and causing the capacity fade with each subsequent charge and discharge cycle.

The combination of computational modelling and experimental characterization was key to this work, Miliante says.

“The way we were able to combine two very different worlds in atomistic modelling and characterization techniques is very new, very different,” says Miliante. “Being able to combine these two worlds is not something you see every day, but at McMaster we have the facilities, the researchers and the willingness to partake in these interdisciplinary collaborations to make it happen.”

An important first step

This understanding of how materials work inside a zinc-ion battery suggests the possibility of new design approaches that can reduce the battery’s capacity fade.

Because researchers now know more about why capacity fades, they can investigate introducing new elements into the material’s internal structure to make it more stable and reduce manganese loss during the charge and discharge cycles.

And thanks to their interdisciplinary approach, they can now screen potential elements and identify new materials that may be less susceptible to manganese dissolution before those materials are synthesized and tested experimentally.

For Miliante, this work fundamentally advances our knowledge of how zinc-ion batteries work and is an important first step towards making these promising batteries a reality.

“In a way, understanding why the capacity fade is happening gives you an indication of how you can fix it,” says Miliante. “It’s like understanding how a motor works, so now you can design better motors.”

Smoke billows out of an industrial smoke stack into a blue sky.

Second life: How McMaster researchers are using copper wires to convert carbon emissions into useful chemicals

Ashkan Irannezhad, a postdoctoral fellow in Drew Higgins’ lab, has discovered a green way to turn captured carbon emissions into ethylene.  
Two men wearing life jackets stand in a river, gathering a sample of water.

McMaster team investigates how ‘forever chemicals’ travel to the Great Lakes  

A research team has received $200,000 in federal funding to better understand how PFAS travel through soils and waterways.
An aerial image from a distance of the countryside around a nuclear power plant and its four smokestacks.

Corrosion control: Expert Suraj Persaud on extending and strengthening Canada’s nuclear enterprise

The Materials Science and Engineering professor explains how his work on corrosion is helping Canada safely and sustainably meet growing demand for nuclear energy.